Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 5.08 - 76.2 microns | 0.200 - 3.00 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.8 |
Sinotek Materials D Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 50.8 - 76.2 microns | 2.00 - 3.00 mil | Side 1 |
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 25.4 - 76.2 microns | 1.00 - 3.00 mil | Side 1 |
Arlon R33670N004 0.004" (0.102 mm) Uncured Silicone Rubber with K2030 PEN Film Substrate Design/Construction:Side 1: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inf.. |
|||
Thickness | 8.00 - 76.2 microns | 0.315 - 3.00 mil | Average value: 31.0 microns Grade Count:152 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Thickness | 38.1 - 76.2 microns | 1.50 - 3.00 mil | Side 1 |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Thickness | 38.1 - 76.2 microns | 1.50 - 3.00 mil | Side 2 |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |