Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 76.0 microns | 0.500 - 2.99 mil | Recommended range for processing |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |