Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 70LTR742 OPP Film Product Description: A matte finish, coated, white, polypropylene film designed for use in demanding thermal transfer, pressure-sensitive label applications. It is also compatible with a wide range .. |
|||
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 60MH247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented PP film. This opaque and stiff film is ideal for mono material requirements and it has been designed for cold s.. |
|||
Thickness | 61.0 microns | 2.40 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 60LH538 OPP Film Product Description: A super white opaque polypropylene film face stock with a proprietary caviated core providing high yield and excellent opacity. The coated print surface provides exceptional ink.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3652 |
3M 3369 General Purpose Aluminum Foil Tape Thinnest aluminum foil tape. UL 723 Classified.Information provided by 3M |
|||
Thickness | 61.0 microns | 2.40 mil | Glass Cloth Backing; ASTM D3752 |
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape 3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 616 Lithographers Tape 3M™ Lithographers Tape 616 is an optically transparent and photographically opaque tape.Information provided by 3M |
|||
Thickness | 61.0 microns | 2.40 mil | Total |
3M CN-3490 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM071 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM111 Indoor UL Recognized Brushed Silver Polyester Label Products 3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM452 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP024901 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP080 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP08R2 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FP101 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FV091 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FV291 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M OFM0101 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M PS191 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3652 |
3M Scotch® 681 Transparent Film Tape Scotch® Tape 681 is an excellent high tack, transparent film tape used for various packaging applications such as temporary holding, combining, light-duty carton sealing, bag sealing, and attaching.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3652 |
3M Scotch® 823 BriteGard™ Film Tape Scotch® BriteGard™ Film Tape 823 bright yellow film tape with a tough 3M™ Scotchpro™ backing is used for label protection. The bright color highlights the packing list or address label for quic.. |
|||
Thickness | 61.0 microns | 2.40 mil | wet film thickness |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Thickness | 61.0 microns | 2.40 mil | estimated wet film thickness |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8403 Polyester Tape 3M™ Polyester Tape 8403 has a silicone adhesive for composite bonding and splicing of many silicone coated papers and films.Information provided by 3M |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8901 Polyester Tape 3M™ Polyester Tape 8901 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FA031 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM291 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FS501 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Thickness | 61.0 microns | 2.40 mil | Total; ASTM D3752 |
3M 8991L Polyester Tape 3M™ Polyester Tape 8991L is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag se.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FM021 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 61.0 microns | 2.40 mil | Liner |
3M FV016401 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |