Physical Properties Metric English Comments
Thickness 60.0 microns
2.36 mil
Average value: 60.0 microns Grade Count:4
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Thickness 60.0 microns
2.36 mil
± 3.0%; ASTM-252-78
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm)
PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh..
Thickness 60.0 microns
2.36 mil
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Thickness 60.0 microns
2.36 mil
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1..
Thickness 60.0 microns
2.36 mil
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Thickness 60.0 microns
2.36 mil
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Thickness 60.0 microns
2.36 mil
Total; Standards
CEN® Electronic Material CS Polyimide Tape
CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel..