Physical Properties Metric English Comments
Thickness 4900 microns
193 mil
AZDEL Test
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..