Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1780 - 3300 microns | 70.0 - 130 mil | |
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Thickness | 1780 microns | 70.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF60 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 1780 - 3300 microns | 70.0 - 130 mil | |
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Thickness | 1780 - 3300 microns | 70.0 - 130 mil | |
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Thickness | 1780 microns | 70.0 mil | ASTM D3652 |
3M Tartan™ 860 Strapping Tape The polypropylene backing of Tartan™ Strapping Tape 860 provides abrasion, moisture and scuff resistance. The adhesives is specifically formulated to provide good adhesion to metallic, plastic, fib.. |
|||
Thickness | 1780 - 3300 microns | 70.0 - 130 mil | |
Zircar Zirconia ZYF-100 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |