Physical Properties Metric English Comments
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4201 General Application Gasketing
Synthetic FiberNitrile BinderExcellent Resistance to Oil & SolventsGood Anti-Stick PropertiesExcellent OEM MaterialInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4300 General Application Gasketing
Synthetic FiberNitrile BinderGood SealabilityGood Chemical ResistanceGeneral Purpose SheetInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4401 General Application Gasketing
Synthetic FiberNitrile BinderExcellent SealabilityExcellent Chemical ResistanceGood Creep RelaxationGeneral Purpose SheetData for this material is available for download into ANSYS xml format: C4401..
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4409 Metal Reinforced Gasketing
Synthetic FiberNitrile BinderHigh Temperature & StressExcellent in Hot GasesReplaces Spiral WoundsVibrationGalvanized Low Carbon Steel InsertInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4430 Compressed Inorganic Fiber Gasketing
Synthetic FiberNitrile BinderExcellent Steam SheetExcellent Chemical ResistanceGood Creep RelaxationGeneral Purpose SheetInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4433 Compressed Inorganic Fiber Sheet
Fiberglass, Aramid & Inorganic FibersNitrile BinderUltimate Steam SheetOutstanding Load BearingExcellent Creep RelaxationBest General Purpose SheetInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4439 Metal Reinforced Gasketing
Fiberglass, Aramid & Inorganic FibersNitrile BinderHigh Temperature & StressVibrationGalvanized Low Carbon Steel InsertInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4500 Carbon Fiber Reinforced Gasketing
Carbon FiberNitrile BinderHigh TemperatureHigh Internal PressureSuitable for a Wide Range of Chemical ApplicationsGood Steam SheetInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4509 Metal Reinforced Gasketing
Carbon FiberNitrile BinderGood in High Load ApplicationsVibrationGalvanized Low Carbon Steel InsertInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-5400 Neoprene Gasketing
Synthetic FiberNeoprene BinderChemically StableGood Anti-Stick PropertiesInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-6327 SBR Binder Gasketing
Synthetic FiberModified SBR BinderControlled SwellUse for Low Temperatures and Low PressuresGood with Low Bolt LoadsInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-6400 SBR Binder Gasketing
Synthetic FiberModified SBR BinderGood Anti-Stick PropertiesGood Steam SheetInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-7400 Chemical Resistant Gasketing
Synthetic FiberEPDM BinderModerate Caustics and AcidsGood Oil Swell CharacteristicsExcellent Aging PropertiesGood in Light Duty SteamInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-8200 Chemical Resistant Gasketing
Synthetic FiberHypalon® BinderAcid ResistantGood Oil-Fuel ResistanceGood Gas SealabilityNo Color AddedInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
+/- 5% of nominal thickness
Thermoseal Miliam Mica PPS 300 Laminate
Type PSSHigh Quality Mica SheetLaminated on Pegged Stainless Steel Insert All Milam laminates are suitable for use in hot, dry gas applications such as exhaust manifolds, turbines, turbo chargers an..
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal ML-5270 PTG Gasketing
Thermoseal ML-5270 is a high performance synthetic fiber and polychloroprene binder gasket material that is resistant to refrigerants and oil mixtures. Its unique Multi-Layer Technology structure pr..
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4324 Compressed Inorganic Fiber Gasketing
Recycled Fiberglass & Aramid BlendNitrile BinderLow Pressure Steam, Water & GasesGood for Oils and FuelsInformation provided by Thermoseal Inc.
Thickness 1588 microns
62.52 mil
Thickness tested
Thermoseal KLINGERSIL® C-4408 Metal Reinforced Gasketing
Synthetic FiberNitrile BinderHigh Temperature & StressFluctuating Temperatures & PressuresVibrationLow Carbon Steel Woven Mesh InsertInformation provided by Thermoseal Inc.