Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1040 microns | 41.0 mil | Total Pad; ASTM D3652 |
3M 5850 Clean-View Pad 3M™ Clean-View Pad 5850 is an adhesive coated polyethylene film layered to form a pad of 20 removable sheets and designed for protection of windows and light fixtures from dirt and from chemical or.. |
|||
Thickness | 1040 - 1240 microns | 41.0 - 49.0 mil | Overall |
Arlon R33682C045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Infor.. |