Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.800 - 1.80 microns | 0.0315 - 0.0709 mil | |
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |