Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 20.0 - 38.1 microns | 0.787 - 1.50 mil | Average value: 27.6 microns Grade Count:12 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Thickness | 25.4 - 38.1 microns | 1.00 - 1.50 mil | Side 1 |
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 25.4 - 38.1 microns | 1.00 - 1.50 mil | Side 2 |
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 25.4 - 38.1 microns | 1.00 - 1.50 mil | Average value: 32.9 microns Grade Count:11 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |