Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.320 - 0.440 microns | 0.0126 - 0.0173 mil | |
Dow Corning FOX® PMCP23 Flowable Oxide Spin-on dielectric (HSQ)Information provided by Dow Corning |
|||
Thickness | 0.305 - 0.440 microns | 0.0120 - 0.0173 mil | 2000-4000 rpm |
Dow SiLK™ I 360 Semiconductor Dielectric Resin SiLK™ I 360 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 360 is compatible with.. |