Polymer Property : Thickness = 0.320 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.320 - 0.440 microns
0.0126 - 0.0173 mil
Dow Corning FOX® PMCP23 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning