Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 900 g/10 min @Load 2.16 kg, Temperature 230 °C |
900 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HF461X Fiber (Melt-blown) Grade Polypropylene Addiform Moplen HF461X is the homopolymer particularly suitable for melt-blown non-woven. It has very high melt flow and narrow molecular weight distribution which promotes thread line continuity an.. |
|||
Melt Flow | 900 g/10 min @Load 2.16 kg, Temperature 190 °C |
900 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil EN 33900 Ethylene n-Butyl Acrylate Copolymer Resin Product Description: ExxonMobil EN 33900 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive.. |