Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.6 g/10 min @Load 5.00 kg, Temperature 250 °C |
9.6 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Melt Flow | 9.6 g/10 min @Load 5.00 kg, Temperature 250 °C |
9.6 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Melt Flow | 9.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin Standard injection molding grade that has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, electric, electronic, medical, safety a.. |
|||
Melt Flow | 9.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® L-1250Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has normal fluidity and weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, elect.. |
|||
Melt Flow | 9.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon TA 2321 HD Red Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2321 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Melt Flow | 9.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® LV-2250Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required for normal fluidity.Applications:.. |
|||
Melt Flow | 9.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® LV-2250Z Transparent and Weather Resistant grade Polycarbonate Resin Typical injection molding grade that has weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of electric, electronic, business machine and industrial equipment com.. |
|||
Melt Flow | 9.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex TEKRON® 4300LM-P96-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 9.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® PM460-H TPC-ET Injection Molding, Heat Stabilized |