Polymer Property : Melt Flow = 9.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Melt Flow 9.4 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.4 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Melt Flow 9.4 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.4 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Melt Flow 9.4 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.4 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Melt Flow 9.4 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.4 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.