Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.1 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.1 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ FR PP Concentrate 4 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Melt Flow | 9.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ FR PE 112 LDPE
(discontinued **) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Melt Flow | 9.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M3007-P Polyethylene
(discontinued **) M3007-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3007-P Has been found to exhibit good barrier properties, temperature resistance, and.. |
|||
Melt Flow | 9.1 g/10 min @Load 10.0 kg, Temperature 250 °C |
9.1 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2734 PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1 |
|||
Melt Flow | 9.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Melt Flow | 9.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Melt Flow | 9.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us.. |