Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.8 g/10 min | 8.8 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 9402-SR BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 8.8 g/10 min | 8.8 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont DGDP-2485 High Density Polyethylene Resin Pétromont® DGDP-2485 Natural is a high density polyethylene copolymer produced using the UNIPOL® process technology. DGDP-2485 is a high performance resin with very high melt strength, excellent .. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SV-0165 U ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SV-0165 U ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Melt Flow | 8.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Melt Flow | 8.8 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.8 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |
|||
Melt Flow | 8.8 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.8 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Dry) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |