Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Melt Flow | 8.3 g/10 min | 8.3 g/10 min | Melt Flow Ratio (I10/I2) is 7.2; ASTM D1238 |
Huntsman Rexell® H2105 Injection Molding LLDPE
(discontinued **) Linear-low high density, injection molding, FDA compliant.Features: High impact strength with reasonable flow.Applications: Articles that must withstand long-term heavy loading such as bottle crates.. |
|||
Melt Flow | 8.3 g/10 min | 8.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in c.. |
|||
Melt Flow | 8.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Centrex® 833 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
Melt Flow | 8.3 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.3 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Melt Flow | 8.3 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.3 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Melt Flow | 8.3 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.3 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Melt Flow | 8.3 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.3 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific) PPE+PS, GF30%, hydrolytic stability improved |
|||
Melt Flow | 8.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and g.. |
|||
Melt Flow | 8.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Melt Flow | 8.3 - 13.8 g/10 min | 8.3 - 13.8 g/10 min | ISO 1133 |
BASF Ecoflex® P BX 7020 Biodegradable Polyester Description: Ecoflex® P BX 7020 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephthalic acid or dimethyltherephthalate i.. |