Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.62 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.62 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon PA 0835 HD Processing Aid Concentrate Masterbatch with a highly effective processing aid for polyethylene, especially PE-HD. By using the PA 0835 HD, the output can be markedly increased and the pressure build-up in the barrel decreased.. |