Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® Elite HH 1891 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos N07N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated and antistatic impact copolymer polypropylene for injection molding applications that require a superior stiffness to impact balance.ApplicationsMaterials .. |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) 6070EA High Density Polyethylene HD6070EA is a high density polyethylene with a narrow molecular weight distribution. It is suitable for a wide range of injection molding applications. This grade has following characteristics: easy.. |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 250 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR11D625 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals .. |
|||
Melt Flow | 7.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of .. |