Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 6.9 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.0 - 6.9 g/10 min
4.0 - 6.9 g/10 min
ASTM D1238
Shuman 811 Black Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
Melt Flow 4.0 - 6.9 g/10 min
4.0 - 6.9 g/10 min
ASTM D1238
Shuman 881 Grey Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
Copyright © lookpolymers.com All Rights Reserved