Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 58 g/10 min @Load 2.16 kg, Temperature 380 °C |
58 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Melt Flow | 58 g/10 min @Load 10.0 kg, Temperature 380 °C |
58 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7107 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Melt Flow | 58 g/10 min @Load 2.16 kg, Temperature 380 °C |
58 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Melt Flow | 58 g/10 min @Load 1.20 kg, Temperature 300 °C |
58 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin Overview: CALIBREâ„¢ 301-58 LT is a high light transmission, high-flow polycarbonate resin for injection molding applications.Main Characteristics:High light transmissionHigh flow for injection m.. |
|||
Melt Flow | 58 g/10 min @Load 1.20 kg, Temperature 300 °C |
58 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133; ASTM D1238 |
Styron CALIBRE™ 1060 DVD Polycarbonate Resin Overview: CALIBRE™ 1060 DVD is a resin that has been developed to address the high demands of the modern optical media industry and is suitable for molding all major disc formats – such as.. |
|||
Melt Flow | 58 g/10 min @Load 2.16 kg, Temperature 230 °C |
58 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 50 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 58 g/10 min @Load 2.16 kg |
58 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.8. |
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It.. |
|||
Melt Flow | 58 g/10 min @Load 10.0 kg, Temperature 380 °C |
58 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7107/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |