Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 53 g/10 min @Load 5.00 kg, Temperature 190 °C |
53 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 57 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Melt Flow | 53 g/10 min | 53 g/10 min | ASTM D1238 |
Flint Hills P9H8M-015 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Melt Flow | 53 g/10 min | 53 g/10 min | ASTM D1238 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 53 g/10 min @Load 2.16 kg, Temperature 230 °C |
53 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H53N-00 Polypropylene Homopolymer This is a high flow rate nucleated and lightly lubricated homopolymer polypropylene designed for high-speed injection molding of thin-walled parts requiring good stiffness and fast cycle times. Thi.. |
|||
Melt Flow | 53 g/10 min @Load 5.00 kg, Temperature 260 °C |
53 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 53 g/10 min @Load 10.0 kg, Temperature 220 °C |
53 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 53 g/10 min | 53 g/10 min | ASTM-D1238 |
CTC X-PRO CTC PP1050 Polypropylene Homopolymer X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Melt Flow | 53 g/10 min @Load 2.16 kg, Temperature 230 °C |
53 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Melt Flow | 53 g/10 min @Load 2.16 kg, Temperature 150 °C |
53 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Arkema Group PLATAMID® H106 PA80 Powder Copolyamide Platamid® H106 PA powder is a special purpose, medium melting point, very low viscosity, thermoplastic copolyamide adhesive suitable for thermal bonding and laminating of textile and foam substrate.. |