Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5000 g/10 min @Load 5.00 kg, Temperature 315 °C |
5000 g/10 min @Load 11.0 lb, Temperature 599 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® PR11 Polyphenylene Sulfide (PPS) Ryton® Polyphenylene Sulfide (PPS) resins are available in several grades exhibiting different molecular weights and molecular architecture. Ryton® PPS exhibits excellent thermal stability and.. |
|||
Melt Flow | 5000 g/10 min @Load 5.00 kg, Temperature 315 °C |
5000 g/10 min @Load 11.0 lb, Temperature 599 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide (PPS) Ryton® Polyphenylene Sulfide (PPS) resins are available in several grades exhibiting different molecular weights and molecular architecture. Ryton® PPS exhibits excellent thermal stability and.. |
|||
Melt Flow | 5000 g/10 min @Load 5.00 kg, Temperature 316 °C |
5000 g/10 min @Load 11.0 lb, Temperature 600 °F |
ASTM D1283 |
Solvay Specialty Polymers Ryton® PR11 Polyphenylene Sulfide Resin
(Unverified Data**) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Melt Flow | 5000 g/10 min | 5000 g/10 min | |
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Melt Flow | 5000 g/10 min | 5000 g/10 min | |
Chevron Phillips Ryton® PR11 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |