Polymer Property : Melt Flow = 50.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.400 - 50.0 g/10 min
0.400 - 50.0 g/10 min
Average value: 12.2 g/10 min Grade Count:117
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Melt Flow 5.00 - 50.0 g/10 min
5.00 - 50.0 g/10 min
Average value: 20.0 g/10 min Grade Count:6
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Melt Flow 17.0 - 50.0 g/10 min
17.0 - 50.0 g/10 min
Average value: 27.7 g/10 min Grade Count:10
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Melt Flow 1.00 - 50.0 g/10 min
1.00 - 50.0 g/10 min
Average value: 18.1 g/10 min Grade Count:18
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Melt Flow 2.00 - 50.0 g/10 min
2.00 - 50.0 g/10 min
Average value: 14.8 g/10 min Grade Count:206
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Melt Flow 2.00 - 50.0 g/10 min
2.00 - 50.0 g/10 min
Average value: 17.8 g/10 min Grade Count:16
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..
Melt Flow 1.00 - 50.0 g/10 min
1.00 - 50.0 g/10 min
Average value: 6.53 g/10 min Grade Count:20
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Melt Flow 3.00 - 50.0 g/10 min
3.00 - 50.0 g/10 min
Average value: 9.70 g/10 min Grade Count:8
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Melt Flow 1.10 - 50.0 g/10 min
1.10 - 50.0 g/10 min
Average value: 17.4 g/10 min Grade Count:3
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Melt Flow 15.0 - 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
15.0 - 50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB1511 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 30.0 - 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30.0 - 50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB2691 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (460000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 30.0 - 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30.0 - 50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB7532 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 2.00 - 50.0 g/10 min
2.00 - 50.0 g/10 min
Average value: 6.30 g/10 min Grade Count:67
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
Melt Flow 3.00 - 50.0 g/10 min
3.00 - 50.0 g/10 min
Average value: 17.4 g/10 min Grade Count:12
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Melt Flow 5.00 - 50.0 g/10 min
5.00 - 50.0 g/10 min
Average value: 22.7 g/10 min Grade Count:3
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..