Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.6 g/10 min | 5.6 g/10 min | ISO 1133:1997 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melt Flow | 5.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
Melt Flow | 5.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Melt Flow | 5.6 g/10 min @Load 10.0 kg, Temperature 230 °C |
5.6 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Ineos ABS Centrex® 401 AES Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Flow | 5.6 g/10 min | 5.6 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA217000 Low Density Polyethylene ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed.. |
|||
Melt Flow | 5.6 g/10 min | 5.6 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Melt Flow | 5.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 5.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Melt Flow | 5.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EC4041AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4041 is recommended for use in the boardstock coating industry. The resin has low neck-in and good drawdown characteristics. Coatings produced from EC4041 have ex.. |
|||
Melt Flow | 5.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® A560 Polymer Modifier DuPont™ Fusabond® A560 is a chemically modified ethylene acrylate copolymer Used as a polymer modifier |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Melt Flow | 5.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
5.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Melt Flow | 5.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
5.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Melt Flow | 5.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman D4041-P Polyethylene
(discontinued **) Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an.. |
|||
Melt Flow | 5.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer