Polymer Property : Melt Flow = 5.40 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Terraloy™ MB 13000A Thermoplastic Starch + PP
Notes: Terraloy™ MB-13000A is a Thermoplastics Starch/PP masterbatch that contains up to 50% of TPS renewable content. Impact PP Melt Index in the masterbatch is 20. This compound is for injectio..
Copyright © lookpolymers.com All Rights Reserved