Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TE-0546-GBK Hexene MDPE Extrusion Resin Very good impact, Excellent ESCR, Sub 50 mesh particles sizeApplications: Powder coating of pipes, values, and fittings to produce a corrosion-resistant coating for buried pipe systemsAdditives: Ant.. |
|||
Melt Flow | 5.1 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.1 g/10 min @Load 47.6 lb, Temperature 302 °F |
Internal Method |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Melt Flow | 5.1 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.1 g/10 min @Load 47.6 lb, Temperature 302 °F |
Internal Method |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Melt Flow | 5.1 g/10 min @Load 10.0 kg, Temperature 250 °C |
5.1 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Melt Flow | 5.1 g/10 min @Load 10.0 kg, Temperature 250 °C |
5.1 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Melt Flow | 5.1 g/10 min @Load 10.0 kg, Temperature 250 °C |
5.1 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Melt Flow | 5.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem CRS5211 PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th.. |
|||
Melt Flow | 5.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Melt Flow | 5.1 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.1 g/10 min @Load 47.6 lb, Temperature 302 °F |
ASTM D1238 |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Melt Flow | 5.1 g/10 min @Load 21.6 kg, Temperature 150 °C |
5.1 g/10 min @Load 47.6 lb, Temperature 302 °F |
ASTM D1238 |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Melt Flow | 5.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex.. |