Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42.7 g/10 min @Load 5.00 kg, Temperature 275 °C |
42.7 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3ZG3 BK 30564 15% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 15% glass fiber reinforced injection-molding grade, for instance, for automotive cable conduits.Information provided by BASF |
|||
Melt Flow | 42.7 g/10 min @Load 5.00 kg, Temperature 275 °C |
42.7 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |