Polymer Property : Melt Flow = 38.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 38.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
S&E Specialty Polymers TufFill™ 5004UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..