Polymer Property : Melt Flow = 35.25 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 35.25 g/10 min

@Load 2.16 kg,
Temperature 250 °C
35.25 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT
Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door ..