Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
33.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 30 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 33.3 g/10 min @Load 5.00 kg, Temperature 275 °C |
33.3 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Melt Flow | 33.3 g/10 min @Load 5.00 kg, Temperature 275 °C |
33.3 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |