Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 32 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 22 - 32 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 - 32 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Melt Flow 18 - 32 g/10 min

@Load 2.16 kg,
Temperature 235 °C
18 - 32 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax CCP PBT 1100-104S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Melt Flow 28 - 32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
28 - 32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Breplast Bretene PP Plus Polypropylene Composite
Recovered polypropylene compositeInformation provided by Breplast S.p.A.