Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 300 g/10 min @Load 2.16 kg |
300 g/10 min @Load 4.76 lb |
|
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA) PRIMACOR® 5980I dispersible polymer is an ethylene acrylic acid copolymer (20 wt % comonomer) which is dispersible in aqueous alkali and amines. Excellent adhesion to metallic, cellulosic, glass an.. |