Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 30.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.00 - 30.0 g/10 min
5.00 - 30.0 g/10 min
Average value: 11.6 g/10 min Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Melt Flow 0.600 - 30.0 g/10 min
0.600 - 30.0 g/10 min
Average value: 12.6 g/10 min Grade Count:268
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Melt Flow 1.00 - 30.0 g/10 min
1.00 - 30.0 g/10 min
Average value: 11.3 g/10 min Grade Count:54
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Melt Flow 0.0570 - 30.0 g/10 min
0.0570 - 30.0 g/10 min
Average value: 7.64 g/10 min Grade Count:22
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Melt Flow 10.0 - 30.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
10.0 - 30.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB0051 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 10.0 - 30.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
10.0 - 30.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB1512 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (350000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro..
Melt Flow 10.0 - 30.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10.0 - 30.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Sinpolene MBW1475 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor ..
Melt Flow 10.0 - 30.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.0 - 30.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene MBW5335 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (200000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 10.0 - 30.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10.0 - 30.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Sinpolene MBW5365 Specialty Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor ..
Melt Flow 10.0 - 30.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
10.0 - 30.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB0061 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 0.200 - 30.0 g/10 min
0.200 - 30.0 g/10 min
Average value: 5.94 g/10 min Grade Count:79
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
Melt Flow 1.00 - 30.0 g/10 min
1.00 - 30.0 g/10 min
Average value: 10.1 g/10 min Grade Count:156
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Melt Flow 2.00 - 30.0 g/10 min
2.00 - 30.0 g/10 min
Average value: 16.9 g/10 min Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Melt Flow 5.50 - 30.0 g/10 min
5.50 - 30.0 g/10 min
Average value: 12.5 g/10 min Grade Count:4
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
Melt Flow 1.00 - 30.0 g/10 min
1.00 - 30.0 g/10 min
Average value: 6.99 g/10 min Grade Count:66
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..
Melt Flow 0.350 - 30.0 g/10 min
0.350 - 30.0 g/10 min
Average value: 11.6 g/10 min Grade Count:6
Overview of materials for Polypropylene w/ 50% Calcium Carbonate
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and ..
Copyright © lookpolymers.com All Rights Reserved