Melt Flow 30.0 g/10 min

@Load 4.90 kg,
Temperature 200 °C
30.0 g/10 min

@Load 10.8 lb,
Temperature 392 °F
ASTM D1238
S&E Specialty Polymers TufPrene™ 2000-40 SEBS
Application: TufPrene 2000-40 is a member of our “unfilled” standard SEBS product line, which ranges from 30 to 90 Shore A. It is a general purpose material designed primarily for injection moldin..
Melt Flow 30.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
30.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1579D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
30.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Monprene® MP-1709A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1775A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2581A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 30.0 - 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30.0 - 50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB2691 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (460000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 30.0 - 50.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30.0 - 50.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB7532 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 30.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
30.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Melt Flow 30.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 30.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade
Super High Gloss, Medium ImpactInformation provided by Bhansali
Melt Flow 30.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Santron IMS 2006 SAN Resin
Very High Rigidity Clear SANInformation provided by Bhansali
Melt Flow 30.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Santron IMS 2006 SAN Resin
Very High Rigidity Clear SANInformation provided by Bhansali
Melt Flow 30.0 - 120 g/10 min
30.0 - 120 g/10 min
Average value: 63.3 g/10 min Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Melt Flow 30.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade
Super High Gloss, Medium ImpactInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved