Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 30.0 g/10 min | 5.00 - 30.0 g/10 min | Average value: 11.6 g/10 min Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Melt Flow | 0.600 - 30.0 g/10 min | 0.600 - 30.0 g/10 min | Average value: 12.6 g/10 min Grade Count:268 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Melt Flow | 1.00 - 30.0 g/10 min | 1.00 - 30.0 g/10 min | Average value: 11.3 g/10 min Grade Count:54 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Melt Flow | 0.0570 - 30.0 g/10 min | 0.0570 - 30.0 g/10 min | Average value: 7.64 g/10 min Grade Count:22 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
10.0 - 30.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB0051 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
10.0 - 30.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1512 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (350000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 - 30.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1475 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor .. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 - 30.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW5335 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (200000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 - 30.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW5365 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor .. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
10.0 - 30.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB0061 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 0.200 - 30.0 g/10 min | 0.200 - 30.0 g/10 min | Average value: 5.94 g/10 min Grade Count:79 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 1.00 - 30.0 g/10 min | 1.00 - 30.0 g/10 min | Average value: 10.1 g/10 min Grade Count:156 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Melt Flow | 2.00 - 30.0 g/10 min | 2.00 - 30.0 g/10 min | Average value: 16.9 g/10 min Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Melt Flow | 5.50 - 30.0 g/10 min | 5.50 - 30.0 g/10 min | Average value: 12.5 g/10 min Grade Count:4 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Melt Flow | 1.00 - 30.0 g/10 min | 1.00 - 30.0 g/10 min | Average value: 6.99 g/10 min Grade Count:66 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Melt Flow | 0.350 - 30.0 g/10 min | 0.350 - 30.0 g/10 min | Average value: 11.6 g/10 min Grade Count:6 |
Overview of materials for Polypropylene w/ 50% Calcium Carbonate This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and .. |