Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 504P Polypropylene Homopolymer for Raffia Applications Product Description: PP 504P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Melt Flow | 3.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D-1238 |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
GRECO ISOPAK 540 ABS Resin Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 3.2 - 4.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 - 4.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem MB 0434 LS-L MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Melt Flow | 3.2 - 4.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 - 4.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Melt Flow | 3.2 g/10 min | 3.2 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) T 30 S Polypropylene T30S is a polypropylene homopolymer particularly suitable for the extrusion of sheet for thermoforming, film yarn and mono filament.Applications: T30S is designed for bags industrial fabrics and mat.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ S10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as .. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Unipetrol PP MONSTEN® TB 003 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Unipetrol PP MONSTEN® TL 003 Polypropylene Homopolymer Made for tape applications. UV stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melt Flow | 3.2 g/10 min | 3.2 g/10 min | ASTM D1238, L |
Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin Clarity. TOTAL Polypropylene M3382MZ produces thermoformed parts with superior clarity, gloss and excellent side wall stiffness.Recommended Applications. TOTAL Polypropylene M3382MZ is ideal for d.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Melt Flow | 3.2 g/10 min | 3.2 g/10 min | Condition G; ASTM D1238 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |