Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 3.1 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.1 g/10 min
3.1 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE G 7940 GRAPHITE
Ash is 7.3%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 3.1 g/10 min
3.1 g/10 min
ASTM D1238
ExxonMobil Escorene® LD 767.MJ Blown Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Melt Flow 3.1 g/10 min
3.1 g/10 min
ASTM D1238
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Melt Flow 3.1 g/10 min
3.1 g/10 min
ASTM D1238
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin  (discontinued **)
Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Melt Flow 3.1 g/10 min
3.1 g/10 min
Exxon Method
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..
Melt Flow 3.1 g/10 min
3.1 g/10 min
ASTM D1238
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
Melt Flow 3.1 - 3.5 g/10 min

@Load 2.61 kg,
Temperature 190 °C
3.1 - 3.5 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC BS500 LDPE
Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical
Melt Flow 3.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ineos Styrenics Polystyrene 476M (NAFTA)
High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF ..
Melt Flow 3.1 g/10 min

@Load 6.60 kg,
Temperature 337 °C
3.1 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 4000 PEI
Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing.
Melt Flow 3.1 g/10 min

@Load 6.60 kg,
Temperature 337 °C
3.1 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific)
Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing.
Melt Flow 3.1 g/10 min

@Load 6.60 kg,
Temperature 337 °C
3.1 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM CRS5201R PEI
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming.
Melt Flow 3.1 g/10 min

@Load 6.60 kg,
Temperature 337 °C
3.1 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific)
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming.
Melt Flow 3.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Styrolution PS 6200/6201 HIPS
Excellent toughnessDesigned for deep draw thermoformingUSP Class VI certifiedInformation provided by Styrolution
Melt Flow 3.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238; ISO 1133
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Melt Flow 3.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Melt Flow 3.1 g/10 min

@Load 2.16 kg,
Temperature 235 °C
3.1 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238R
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Melt Flow 3.1 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.1 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me..
Melt Flow 3.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Melt Flow 3.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Melt Flow 3.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Melt Flow 3.1 g/10 min

@Load 10.0 kg,
Temperature 235 °C
3.1 g/10 min

@Load 22.0 lb,
Temperature 455 °F
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res..
Melt Flow 3.1 g/10 min

@Load 10.0 kg,
Temperature 235 °C
3.1 g/10 min

@Load 22.0 lb,
Temperature 455 °F
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res..
Melt Flow 3.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck..
Copyright © lookpolymers.com All Rights Reserved