Physical Properties Metric English Comments
Melt Flow 22 - 28 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 - 28 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 4340R (EP2Z29G) Propylene and Ethylene Copolymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Melt Flow 22 - 28 g/10 min

@Load 3.80 kg,
Temperature 230 °C
22 - 28 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced
Information provided by Ravago.
Melt Flow 14 - 28 g/10 min

@Load 5.00 kg,
Temperature 230 °C
14 - 28 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Kraton® FG1901 G (SEBS) grafted with MA
Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id..
Melt Flow 14 - 28 g/10 min

@Load 5.00 kg,
Temperature 230 °C
14 - 28 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Kraton® FG1901 G (SEBS) Linear Block Copolymer
Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id..
Melt Flow 14 - 28 g/10 min

@Load 5.00 kg,
Temperature 230 °C
14 - 28 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Kraton® FG1901 G (SEBS) grafted with MA
Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form i..
Melt Flow 22 - 28 g/10 min

@Load 5.00 kg,
Temperature 372 °C
22 - 28 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Melt Flow 20 - 28 g/10 min

@Load 5.00 kg,
Temperature 365 °C
20 - 28 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Melt Flow 24 - 28 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 - 28 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang.
Melt Flow 22 - 28 g/10 min

@Load 5.00 kg,
Temperature 372 °C
22 - 28 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
Melt Flow 22 - 28 g/10 min

@Load 3.80 kg,
Temperature 230 °C
22 - 28 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Melt Flow 18 - 28 g/10 min
18 - 28 g/10 min
ISO 1133
Beijing Ranger Chem BLUESTAR® 1110 PBT
Can be used directly for spinning, or it can be used after reinforcement & compounding. It can also be used to produce cable sheath through tackificationInformation provided by Beijing Ranger Chemic..
Melt Flow 7.0 - 28 g/10 min

@Load 12.5 kg,
Temperature 232 °C
7.0 - 28 g/10 min

@Load 27.6 lb,
Temperature 450 °F
ASTM D1238
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Melt Flow 25 - 28 g/10 min
25 - 28 g/10 min
Ashley Polymers Ashlene® R195B Acetal
A general purpose, low viscosity with excellent toughness, strength, stiffness, lubricity in black. Available in UV stabilized grades: R195-B2 (good weatherability); R195-HB2 (maximum weatherabili..
Melt Flow 24.1 - 28 g/10 min
24.1 - 28 g/10 min
C
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff..