Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24 - 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 - 26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 24 - 26 g/10 min | 24 - 26 g/10 min | ASTM D1238 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 24 - 26 g/10 min | 24 - 26 g/10 min | ASTM D1238 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 18 - 26 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 - 26 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kureha KF Polymer 850 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melt Flow | 20 - 26 g/10 min | 20 - 26 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D0850 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |