Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24.65 g/10 min @Load 2.16 kg, Temperature 250 °C |
24.65 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Melt Flow | 24.65 g/10 min @Load 2.16 kg, Temperature 275 °C |
24.65 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |