Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
24.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Melt Flow | 24.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
24.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical SEETEC H7630 Polypropylene, Homopolymer Features: Seetec H7630 is designed for the extrusion of continuous filament (CF) & bulk continuous filament (BCF) fibers and staple fibers. This grade is characterized by medium MWD, with anti-gas f.. |