Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.800 - 22.0 g/10 min | 0.800 - 22.0 g/10 min | Average value: 5.88 g/10 min Grade Count:27 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 502 Black Polypropylene Copolymer Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 502C Black Polypropylene Copolymer Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |
|||
Melt Flow | 0.250 - 22.0 g/10 min | 0.250 - 22.0 g/10 min | Average value: 2.50 g/10 min Grade Count:40 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Melt Flow | 9.00 - 22.0 g/10 min | 9.00 - 22.0 g/10 min | Average value: 16.4 g/10 min Grade Count:8 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |