Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 21.45 g/10 min @Load 2.16 kg, Temperature 300 °C |
21.45 g/10 min @Load 4.76 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |