Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 21.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
21.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2880E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 21.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
21.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Melt Flow | 21.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
21.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |