Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Polimeri Europa Dutral® PM 8273 Ethylene - Propylene Masterbatch Dutral® PM 8273 is a masterbatch based on Ethylene - Propylene elastomer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the produc.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 300 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 90-0304 Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 - 3.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 - 3.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1500J (T30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Yparex® 8403 R Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melt Flow | 2.4 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
GRECO ISOPAK 547M ABS Resin Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 2.4 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 5310 HIPS Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis SuperCOPO™ LE4205R Polyethylene Insulation Compound, Crosslinkable SuperCOPO™ LE4205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LE4205R is intended for insulation of XLPE power cabl.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers TR 5000 AS/P Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.4 g/10 min | 2.4 g/10 min | Condition E; ASTM D 1238 |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® 9000 HDC N 123 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |