Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Polimeri Europa Dutral® PM 8273 Ethylene - Propylene Masterbatch Dutral® PM 8273 is a masterbatch based on Ethylene - Propylene elastomer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the produc.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 300 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 - 3.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 - 3.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1500J (T30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 2.4 g/10 min @Temperature 190 °C |
2.4 g/10 min @Temperature 374 °F |
|
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Yparex® 8403 R Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 400 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 90-0304 F Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Melt Flow | 2.4 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
GRECO ISOPAK 547M ABS Resin Metal Plating GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® G 7705 TPE Styrene Ethylene Butylene Styrene Block Copolymer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron Magnumâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) High Heat, Low Gloss ABS.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis SuperCOPO™ LE4205R Polyethylene Insulation Compound, Crosslinkable SuperCOPO™ LE4205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LE4205R is intended for insulation of XLPE power cabl.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal .. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 2.4 g/10 min | 2.4 g/10 min | Condition E; ASTM D 1238 |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |