Polymer Property : Melt Flow = 17.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 17.0 - 50.0 g/10 min
17.0 - 50.0 g/10 min
Average value: 27.7 g/10 min Grade Count:10
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Melt Flow 17.0 - 22.0 g/10 min
17.0 - 22.0 g/10 min
Shuman 502 Black Polypropylene Copolymer
Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Melt Flow 17.0 - 22.0 g/10 min
17.0 - 22.0 g/10 min
Shuman 502C Black Polypropylene Copolymer
Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Melt Flow 17.0 - 22.0 g/10 min
17.0 - 22.0 g/10 min
Shuman 510 Black Polypropylene Homopolymer
Excellent chemical resistance, excellent processabilityData provided by the manufacturer.
Melt Flow 17.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 17.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
17.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1527 Thermoplastic Elastomer
Notes: Translucent Features: Good Flow; Tough; Good Melt StrengthInformation Provided by Teknor Apex
Melt Flow 17.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
17.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4955A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4985A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4975A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
BASF Ultradur B 4406 G4 PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Melt Flow 17.0 - 52.0 g/10 min
17.0 - 52.0 g/10 min
Average value: 28.5 g/10 min Grade Count:4
Overview of materials for Silicone Polyurethane, Polycarbonate Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim..