Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 15.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 15.3 g/10 min

@Load 6.70 kg,
Temperature 285 °C
15.3 g/10 min

@Load 14.8 lb,
Temperature 545 °F
ASTM D1238
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6
LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant
Melt Flow 15.3 g/10 min

@Load 6.70 kg,
Temperature 285 °C
15.3 g/10 min

@Load 14.8 lb,
Temperature 545 °F
ASTM D1238
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Melt Flow <= 15.3 g/10 min

@Load 5.00 kg,
Temperature 345 °C
<= 15.3 g/10 min

@Load 11.0 lb,
Temperature 653 °F
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL PKN4775 PPE+PS
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Melt Flow 15.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
15.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2907 PPE+PS (Asia Pacific)
PPE+HIPS GF10% FR V-1
Copyright © lookpolymers.com All Rights Reserved